Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.80 GPa | 1280 ksi | |
Plastcom SLOVAMID 6 GF 30 HI PA6, 30% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength a.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527 |
Nilit FRIANYL B63 H-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 8.80 GPa @Temperature 23.0 °C |
1280 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527-2 |
Pasargad Polymer Peyvand Pasamid 3P-H7130B Nylon 6/66, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ASTM D638 |
Plenco 4246 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is use.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527-1/-2 |
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527-1/-2 |
Lanxess Durethan® DP AKV 30 HR EF 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, good heat-ageing resistance and hydrolysis resistance, good flowability (Easy Flow) |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® AKV 40 H3.0 000000 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | |
LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V25 Black 21NHFE PA66, 25% glass fiber, DRY Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10 LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF006EU PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF006EU is a compound based on PA 66 resin containing Glass Fiber. Added features include: Easy Molding, UV-StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ASTM D638 |
Plenco 2369 Phenolic, Granular, Compression Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ASTM D638 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Tensile Modulus | 8.80 GPa @Temperature 160 °C |
1280 ksi @Temperature 320 °F |
ISO 527-1/-2 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide RF006EU PA66/6, Glass Fiber Filled, Injection Molded Staramide RF006EU is an UV stabilized, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66C 30V S4)Information provided by Eurostar. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 6630 Nylon 66 Alloy, 30% Glass Fiber (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527-1, 2 |
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |