Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4246 Phenolic, Granular, Injection Molded  (discontinued **)

Category Polymer , Thermoset , Phenolic , Phenolic, Novolac, Heat Resistant Grade, Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Plenco 4246 Phenolic, Granular, Injection Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-stage Phenolic. PLENCO 04246 flow 18 is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is used in appliance applications and can be molded by compression, transfer, or injection.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Apparent Bulk Density 0.720 g/cc
0.0260 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.26 %
0.26 %
ASTM D570
Linear Mold Shrinkage 0.0081 cm/cm
0.0081 in/in
per ATM D955. Post shrinkage is 0.31% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 79
79
ASTM D785
Tensile Strength, Ultimate 58.9 MPa
8540 psi
ASTM D638
Elongation at Break 0.83 %
0.83 %
ASTM D638
Tensile Modulus 8.80 GPa
1280 ksi
ASTM D638
Flexural Yield Strength 88.5 MPa
12800 psi
ASTM D790
Flexural Modulus 8.16 GPa
1180 ksi
ASTM D790
Compressive Yield Strength 199.1 MPa
28880 psi
ASTM D695
Charpy Impact, Notched 0.170 J/cm²
0.809 ft-lb/in²
ASTM D256
Impact 98
98
J/m Plenco drop ball test
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 201 °C
394 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 169 °C
336 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.18 mm
V-1

@Thickness 0.125 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.35e+11 ohm-cm
1.35e+11 ohm-cm
ASTM D257
Dielectric Constant 5.3

@Frequency 1e+6 Hz
5.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 10.0 kV/mm
254 kV/in
Short Time; ASTM D149
Dissipation Factor 0.068

@Frequency 1e+6 Hz
0.068

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 150 sec
150 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638