Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp RF006EU PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp RF006EU PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* RF006EU is a compound based on PA 66 resin containing Glass Fiber. Added features include: Easy Molding, UV-StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Water Absorption 3.0 %

@Temperature 23.0 °C,
Time 86400 sec
3.0 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 170 MPa
24700 psi
5 mm/min; ISO 527
Elongation at Yield 3.3 %
3.3 %
5 mm/min; ISO 527
Tensile Modulus 8.80 GPa
1280 ksi
1 mm/min; ISO 527
Flexural Yield Strength 233 MPa
33800 psi
2 mm/min; ISO 178
Flexural Modulus 7.60 GPa
1100 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 24.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
13.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af