Material Notes:
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Physical Properties Metric English Comments
Specific Gravity 1.045 g/cc
1.045 g/cc
ASTM D792
Linear Mold Shrinkage 0.00400 - 0.00500 cm/cm
0.00400 - 0.00500 in/in
ASTM D955
Melt Flow 13.0 g/10 min
<br>@Load 10.0 kg,<br> Temperature 220 °C
13.0 g/10 min
<br>@Load 22.0 lb,<br> Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 58.8 MPa
<br>@Thickness 3.20 mm
8530 psi
<br>@Thickness 0.126 in
Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 80.4 MPa
<br>@Thickness 6.40 mm
11700 psi
<br>@Thickness 0.252 in
5 mm/min; ASTM D790
Flexural Modulus 2.75 GPa
<br>@Thickness 6.40 mm
398 ksi
<br>@Thickness 0.252 in
5 mm/min; ASTM D790
Izod Impact, Notched 1.67 J/cm
<br>@Thickness 6.40 mm
3.12 ft-lb/in
<br>@Thickness 0.252 in
ASTM D256
2.26 J/cm
<br>@Thickness 3.20 mm
4.22 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C
<br>@Thickness 6.40 mm
207 °F
<br>@Thickness 0.252 in
Method A; ASTM D648
Flammability, UL94 HB
<br>@Thickness 3.20 mm
HB
<br>@Thickness 0.126 in