Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 82.0 MPa | 11900 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPR-30G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ X MX5210-0030 RS Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ASTM D638 |
Nilit Polynil® P230 High Viscosity Nylon 66 Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KX98009 is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber, Glass Fiber. Added features include : EMI / RFI Shielding, Electrically Conductive. |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ISO 527 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, DAM Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by G.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RX06001 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RX06001 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Easy Molding, High Impact, Electrically Conductive. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific) LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | SABIC - Japan Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific) |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF006I is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Tensile Strength, Yield | 82.0 MPa @Thickness 6.35 mm |
11900 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ISO 527-1/-2 |
Unitika A125 PA66, Dry Information provided by Unitika Ltd. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ASTM-D638 |
Polyram PlusTek PA103 Nylon 6.6, Injection Molding Polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ASTM D638 |
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive) Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | dry; ISO 527-1/-2 |
DSM Novamid® 1013C5 PA6 Injection Molding, Easy Molding Grade |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Strength, Yield | 82.0 MPa @Temperature 23.0 °C |
11900 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® FE3071 NC010 Nylon 66 Zytel® FE3071 NC010 is an intermediate viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | ISO 527 |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
Tensile Strength, Yield | 82.4 MPa | 11900 psi | ASTM D638 |
Cheng Yu Plastic A705G3 ABS 30% Glass Fiber Reinforced |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL PX2935 PPE+PS (Asia Pacific) PPE/PS, GF20%, non-FR |
|||
Tensile Strength, Yield | 82.0 MPa | 11900 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |