| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Novamid® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Novamid® 1013C5 PA6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | dry; ISO 1183 |
| Viscosity Test | 138 cm³/g | 138 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
| Linear Mold Shrinkage, Flow | 0.011 cm/cm | 0.011 in/in | Sim. To ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Sim. To ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 82.0 MPa | 11900 psi | dry; ISO 527-1/-2 |
| Elongation at Break | 19 % | 19 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 3.20 GPa | 464 ksi | dry; ISO 527-1/-2 |
| Flexural Strength | 110 MPa | 16000 psi | dry; ISO 178 |
| Flexural Modulus | 2.80 GPa | 406 ksi | dry; ISO 178 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
dry; ISO 179/1eU |
| Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 169 °C | 336 °F | dry; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 76.0 °C | 169 °F | dry; ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | dry; IEC 60093 |
| Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
| Dielectric Constant | 4.0 @Frequency 100 Hz |
4.0 @Frequency 100 Hz |
dry; IEC 60250 |
| 4.0 @Frequency 1.00e+6 Hz |
4.0 @Frequency 1.00e+6 Hz |
dry; IEC 60250 | |
| Dielectric Strength | 26.0 kV/mm | 660 kV/in | dry; IEC 60243-1 |
| Dissipation Factor | 0.011 @Frequency 100 Hz |
0.011 @Frequency 100 Hz |
dry; IEC 60250 |
| 0.022 @Frequency 1.00e+6 Hz |
0.022 @Frequency 1.00e+6 Hz |
dry; IEC 60250 | |
| Comparative Tracking Index | 600 V | 600 V | dry; IEC 60112 |