Polymer Property : Tensile Strength, Yield = 11900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.0 MPa
11900 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ PPR-30G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 82.0 MPa
11900 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ X MX5210-0030 RS Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
Nilit Polynil® P230 High Viscosity Nylon 66
Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various..
Tensile Strength, Yield 82.0 MPa
11900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East)
LNP* FARADEX* KX98009 is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber, Glass Fiber. Added features include : EMI / RFI Shielding, Electrically Conductive.
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Tensile Strength, Yield 82.0 MPa

@Temperature 23.0 °C
11900 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 - 90.0 MPa
11900 - 13100 psi
Average value: 88.0 MPa Grade Count:5
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Tensile Strength, Yield 82.0 MPa
11900 psi
ISO value at 50 mm/min.
BASF Capron® 8202 NL Nylon 6 (Dry)  (discontinued **)
Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta..
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 82.0 MPa
11900 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
Tensile Strength, Yield 82.0 MPa
11900 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific)
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding.
Tensile Strength, Yield 82.0 MPa
11900 psi
SABIC - Japan Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific)
Tensile Strength, Yield 82.0 MPa
11900 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT (Europe-Africa-Middle East)
LNP* Thermotuf* WF006I is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact.
Tensile Strength, Yield 82.0 MPa

@Thickness 6.35 mm
11900 psi

@Thickness 0.250 in
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Tensile Strength, Yield 82.0 MPa

@Thickness 6.35 mm
11900 psi

@Thickness 0.250 in
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Tensile Strength, Yield 82.0 MPa
11900 psi
ISO 527-1/-2
Unitika A125 PA66, Dry
Information provided by Unitika Ltd.
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM-D638
Polyram PlusTek PA103 Nylon 6.6, Injection Molding
Polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Tensile Strength, Yield 82.0 MPa
11900 psi
ASTM D638
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive)
Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32..
Tensile Strength, Yield 82.0 MPa
11900 psi
dry; ISO 527-1/-2
DSM Novamid® 1013C5 PA6
Injection Molding, Easy Molding Grade
Tensile Strength, Yield 82.0 MPa

@Temperature 23.0 °C
11900 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FE3071 NC010 Nylon 66
Zytel® FE3071 NC010 is an intermediate viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 MPa
11900 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 MPa
11900 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 MPa
11900 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 82.0 MPa
11900 psi
SABIC - Japan Method
SABIC Innovative Plastics NORYL PX2935 PPE+PS (Asia Pacific)
PPE/PS, GF20%, non-FR
Tensile Strength, Yield 82.0 MPa
11900 psi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont ..