| Category | Polymer , Thermoplastic , Polycarbonate (PC) | 
| Manufacturer | SABIC Innovative Plastics (GE Plastics) | 
| Trade Name | LNP THERMOCOMP | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7602 PC (Asia Pacific).pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.28 g/cc | 1.28 g/cc | ASTM D792 | 
| Water Absorption |           0.12 %                     @Time 86400 sec  | 
                  0.12 %                     @Time 24.0 hour  | 
        ASTM D570 | 
| Linear Mold Shrinkage, Flow |           0.0030 - 0.0040           cm/cm           @Thickness 3.20 mm  | 
                  0.0030 - 0.0040           in/in           @Thickness 0.126 in  | 
        SABIC Method | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Yield | 82.0 MPa | 11900 psi | SABIC - Japan Method | 
| Elongation at Break | 10 - 20 % | 10 - 20 % | SABIC - Japan Method | 
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 | 
| Flexural Modulus | 3.92 GPa | 569 ksi | ASTM D790 | 
| Izod Impact, Notched | 0.880 J/cm | 1.65 ft-lb/in | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           40.0 - 60.0           µm/m-°C           @Temperature -30.0 - 30.0 °C  | 
                  22.2 - 33.3           µin/in-°F           @Temperature -22.0 - 86.0 °F  | 
        TMA | 
| Deflection Temperature at 0.46 MPa (66 psi) |           100           °C           @Thickness 3.20 mm  | 
                  212           °F           @Thickness 0.126 in  | 
        unannealed; ASTM D648 | 
| Flammability, UL94 |           V-0                     @Thickness 0.750 mm  | 
                  V-0                     @Thickness 0.0295 in  | 
        UL 94 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |