Polymer Property : Izod Impact, Notched (ISO) = 3.00 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN
High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound
Izod Impact, Notched (ISO) 3.00 kJ/m² - NB
1.43 ft-lb/in² - NB
Average value: 32.8 kJ/m² Grade Count:28
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 3.00 - 14.0 kJ/m²

@Temperature -30.0 - -30.0 °C
1.43 - 6.66 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 7.45 kJ/m² Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched (ISO) 3.00 - 10.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 6.70 kJ/m² Grade Count:14
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched (ISO) 3.00 kJ/m² - NB
1.43 ft-lb/in² - NB
Average value: 12.4 kJ/m² Grade Count:14
Overview of materials for Nylon 66/6
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Izod Impact, Notched (ISO) 3.00 - 8.50 kJ/m²
1.43 - 4.04 ft-lb/in²
Average value: 6.00 kJ/m² Grade Count:3
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Izod Impact, Notched (ISO) 3.00 - 4.00 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 1.90 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.50 kJ/m² Grade Count:1
Overview of materials for Nylon 66, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate..
Izod Impact, Notched (ISO) 3.00 - 20.0 kJ/m²
1.43 - 9.52 ft-lb/in²
Average value: 8.40 kJ/m² Grade Count:37
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East)
LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Lubricomp KZL34 POM
LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180
Solvay TECHNYL® A 718 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL A 718 V30 is a polyamide 66 reinforced with glass fiber and thermal stabilized for injection moldingColors: it is sailed on natural and black colorAvailable in: Latin AmericaMai..
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP Lubricomp ML002S PP
LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP UAL23AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UAL23AS is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include : Internally Lubricated, Heat Stabilized.
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 0.000 °C
1.43 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® 7062HP PBT
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East)
LNP* STAT-KON* PD000 is a compound based on PA 6 resin containing Carbon Powder. Added features include: Electrically Conductive.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Izod Impact, Notched (ISO) >= 3.00 kJ/m²

@Temperature 0.000 °C
>= 1.43 ft-lb/in²

@Temperature 32.0 °F
Sibur 21020-PM1 Polypropylene with Low Haze
For production of three-layer PE/PP film, for production of sheets for cups and thin casting. It is allowed for contact with food products.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP
LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s).
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180-93
Wellman Wellamid® FRGS25-66-NBK3 Nylon 66, 25% Glass Sphere Reinforced, Flame Retardant
All information provided by Wellman Engineered Resins.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180-93
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 179
Total PPH 10042 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad ..
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80x10x4; ISO 179/1eA
Eurostar Staramide RB008 PA66, 40% Glass Bead Filled, Injection Molded
Staramide RB008 is a 40% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
Addiplast Addinyl B2 1 Flame Retardant Nylon 6
Flame retardant, halogen freeInformation provided by Addiplast.
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
Addiplast Addinyl A2 1 Flame Retardant Nylon 66
Flame retardant, halogen freeInformation provided by Addiplast.
Izod Impact, Notched (ISO) 3.00 - 5.90 kJ/m²
1.43 - 2.81 ft-lb/in²
Average value: 4.42 kJ/m² Grade Count:6
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..