Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Moisture Absorption 0.0300 %
0.0300 %
50% RH, 24 hrs; ASTM D570
0.0500 %
0.0500 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow >= 0.020 cm/cm

@Time 86400 sec
>= 0.020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm

@Time 86400 sec
0.010 - 0.030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 76.0 MPa
11000 psi
Type I, 5 mm/min; ASTM D638
76.0 MPa
11000 psi
5 mm/min; ISO 527
Tensile Strength, Yield 77.0 MPa
11200 psi
Type I, 5 mm/min; ASTM D638
77.0 MPa
11200 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
3.0 %
3.0 %
5 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 6.06 GPa
879 ksi
5 mm/min; ASTM D638
6.15 GPa
892 ksi
1 mm/min; ISO 527
Flexural Strength 126 MPa
18300 psi
ISO 178
128 MPa
18600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength 130 MPa
18900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5.67 GPa
822 ksi
2 mm/min; ISO 178
5.73 GPa
831 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.77 J/cm
5.19 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 5.00 J

@Temperature 23.0 °C
3.69 ft-lb

@Temperature 73.4 °F
ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 51.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
28.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
32.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 207 °C
405 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
216 °C

@Thickness 3.20 mm
421 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
185 °C

@Thickness 3.20 mm
365 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: