Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Qualchem Danamid FGF-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Faradex KS003AI Acetal Copolymer (Europe-Africa-Middle East) LNP* FARADEX* KS003AI is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include; EMI/RFI Shielding, Electrically Conductive.This data was supplied by SAB.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL0039E is a compound based on Polycarbonate resin containing PTFE, Flame retardant. Added features include: Easy Molding, Internally Lubricated, Flame retardant. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180/U |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180 |
Qualchem Danamid FGFHUV-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial light.Information provided by Qualchem Zrt. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/U |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 2nd Grade |
Kazanorgsintez PC-007 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12 LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL36 is a compound based on PA 66 resin containing PTFE, Carbon Fiber. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RCL36XXP PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RCL36XXP is a compound based on PA 66 resin, containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP C1000XXP PS (Europe-Africa-Middle East) LNP* THERMOCOMP* C1000XXP is a compound based on Polystyrene resin. Added features include: High Impact. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF00AH PA 66 LNP* THERMOCOMP* RF00AH is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Asia Pacific) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G30 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-MFC-G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² | 28.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RVN17SXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVN17SXS is a compound based on PA 66 resin containing Long Glass Fiber, MoS2. Added features include; Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |