Kazanorgsintez PC-007 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kazanorgsintez PC-007 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Melt Flow 6.0 - 8.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
6.0 - 8.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 55.0 MPa
>= 7980 psi
2nd Grade
>= 58.0 MPa
>= 8410 psi
1st Grade
>= 60.0 MPa
>= 8700 psi
Superior Quality
Elongation at Break >= 80 %
>= 80 %
2nd Grade
>= 100 %
>= 100 %
Superior Quality, 1st Grade
Flexural Modulus 2.00 GPa
290 ksi
2nd Grade
2.25 GPa
326 ksi
Superior Grade, 1st Grade
Transverse Strength >= 70.0 MPa
>= 10200 psi
2nd Grade, at max sample load
>= 80.0 MPa
>= 11600 psi
Superior Quality, 1st Grade, at max sample load
Compressive Yield Strength >= 70.0 MPa
>= 10200 psi
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
2nd Grade
66.0 kJ/m²
31.4 ft-lb/in²
Superior Grade, 1st Grade
Thermal Properties Metric English Comments
Vicat Softening Point >= 147 °C
>= 297 °F
Optical Properties Metric English Comments
Transmission, Visible 85 %
85 %
2nd Grade
89 %
89 %
Superior Quality, 1st Grade
>= 90 %
>= 90 %
Superior Grade, 1st Grade
Electrical Properties Metric English Comments
Dielectric Constant <= 3.1

@Frequency 1000 Hz
<= 3.1

@Frequency 1000 Hz
Superior Quality
Dielectric Strength >= 20.0 kV/mm
>= 508 kV/in
Superior Quality
Dissipation Factor <= 0.0090

@Frequency 1000 Hz
<= 0.0090

@Frequency 1000 Hz
Superior Quality
Descriptive Properties Value Comments
Amount of impurities [pcs] 10
1st Grade
5
Superior Quality
Turbidity 0.8
Superior Grade, 1st Grade
1
2nd Grade