Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | ISO 180 |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature -30.0 °C |
17.6 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH4560 PBT (Asia Pacific) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp WX01910L PBT LNP* Thermocomp* WX01910L is a compound based on Thermoplastic Polyester containing Proprietary Fillers. Characteristics of this grade are: Low Extractable.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP NF001XXX PC+ABS LNP* THERMOCOMP* PCA-F-1001 is a compound based on PC+ABS resin containing 5% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS (Asia Pacific) LNP* Thermocomp* NF004 is a compound based on PC+ABS Blend resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA (Asia Pacific) LNP* Thermocomp* UFW49S is a compound based on Polyphthalamide resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized, Low Warpage. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² | 17.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 37.0 kJ/m² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East) LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 37.0 - 37.0 kJ/m² @Temperature -30.0 - -30.0 °C |
17.6 - 17.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 37.0 kJ/m² Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |