Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
11.4 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 - 33.0 kJ/m² | 11.4 - 15.7 ft-lb/in² | Average value: 28.4 kJ/m² Grade Count:5 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific) LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp OFB32I PPS LNP LUBRICOMP* OFB32I is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SA.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Linear LNP* LUBRICOMP* OFL36 is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66 LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC LNP* Stat-Kon* DEL369E is a compound based on Polycarbonate containing Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant and Statically Conductive.This data was supplied by S.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific) LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC LNP STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.This data was supplied by.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific) LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific) LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RE0029 PA 66 LNP* STAT-KON* RE0029 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | ISO 180 |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |