SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics LNP Stat-kon DEL369E PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Stat-Kon* DEL369E is a Polycarbonate with Carbon Fiber and PTFE. Characteristics of this grade are Flame Retardant.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D 792
Density 1.48 g/cc
0.0535 lb/in³
ASTM D 792
Moisture Absorption at Equilibrium 0.12 %
0.12 %
23°C / 50% RH; ISO 62
0.10 %
<br>@Time 86400 sec
0.10 %
<br>@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.00080 - 0.0010 cm/cm
<br>@Time 86400 sec
0.00080 - 0.0010 in/in
<br>@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0040 cm/cm
<br>@Time 86400 sec
0.0020 - 0.0040 in/in
<br>@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 132 MPa
19100 psi
5 mm/min; ISO 527
133 MPa
19300 psi
Type I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 132 MPa
19100 psi
5 mm/min; ISO 527
133 MPa
19300 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 1.0 %
1.0 %
5 mm/min; ISO 527
1.2 %
1.2 %
Type I, 5 mm/min; ASTM D 638
Elongation at Yield 1.0 %
1.0 %
5 mm/min; ISO 527
1.2 %
1.2 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 21.84 GPa
3168 ksi
1 mm/min; ISO 527
22.6 GPa
3280 ksi
50 mm/min; ASTM D 638
Flexural Strength 123 MPa
17800 psi
ISO 178
196 MPa
28400 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Yield Strength 195 MPa
28300 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 15.76 GPa
2286 ksi
1.3 mm/min, 50 mm span; ASTM D 790
17.21 GPa
2496 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.580 J/cm
<br>@Temperature 23.0 °C
1.09 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 4.08 J/cm
<br>@Temperature 23.0 °C
7.64 ft-lb/in
<br>@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 6.00 kJ/m²
<br>@Temperature 23.0 °C
2.86 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 24.0 kJ/m²
<br>@Temperature 23.0 °C
11.4 ft-lb/in²
<br>@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
11.0 J
<br>@Temperature 23.0 °C
8.11 ft-lb
<br>@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
149 °C
<br>@Thickness 3.20 mm
300 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
143 °C
<br>@Thickness 3.20 mm
289 °F
<br>@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Surface Resistance 1.0 - 3.0 ohm
1.0 - 3.0 ohm
ASTM D 257