| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ASTM D792 |
| Density | 1.196 g/cc | 0.04321 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.0600 % | 0.0600 % | 50% RH, 24 hrs; ASTM D570 |
| 0.210 % | 0.210 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0080 - 0.010 cm/cm @Time 86400 sec |
0.0080 - 0.010 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 47.0 MPa | 6820 psi | Type I, 5 mm/min; ASTM D638 |
| 48.0 MPa | 6960 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 16.3 % | 16.3 % | 5 mm/min; ISO 527 |
| 16.5 % | 16.5 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 12.3 % | 12.3 % | 5 mm/min; ISO 527 |
| 13.7 % | 13.7 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
| 2.49 GPa | 361 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 76.0 MPa | 11000 psi | ISO 178 |
| Flexural Modulus | 2.34 GPa | 339 ksi | 2 mm/min; ISO 178 |
| 2.54 GPa | 368 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.520 J/cm | 0.974 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 3.37 J/cm | 6.31 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 24.0 kJ/m² | 11.4 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 13.0 J @Temperature 23.0 °C |
9.59 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 2.00 J | 1.48 ft-lb | Multiaxial Impact; ISO 6603 |
| Coefficient of Friction, Dynamic | 0.28 | 0.28 | ASTM D3702 Modified |
| Coefficient of Friction, Static | 0.35 | 0.35 | ASTM D3702 Modified |
| K (wear) Factor | 2.01 x 10-8 mm³/N-M | 1.00 x 10-10 in³-min/ft-lb-hr | Ring; ASTM D3702 Modified |
| 145 x 10-8 mm³/N-M | 72.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
42.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 127 °C | 261 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 130 °C @Thickness 3.20 mm |
266 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 114 °C | 237 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |