Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 37.0 kJ/m² | 10.5 - 17.6 ft-lb/in² | Average value: 32.0 kJ/m² Grade Count:3 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 34.0 kJ/m² | 10.5 - 16.2 ft-lb/in² | Average value: 27.8 kJ/m² Grade Count:5 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 27.0 kJ/m² | 10.5 - 12.8 ft-lb/in² | Average value: 24.3 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 27.0 kJ/m² @Temperature -30.0 - -30.0 °C |
10.5 - 12.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 24.3 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This .. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AX06437 ABS LNP* THERMOCOMP* AX06437 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS LNP* THERMOCOMP* AX08306 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this grade is: Platable. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AX08306 ABS (Asia Pacific) LNP* Thermocomp* AX08306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Mineral. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF0081PI PC (Asia Pacific) LNP* Thermocomp* DF0081PI is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, good flatness, Non-Brominated & .. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF002XXH PA 66 LNP THERMOCOMP* RF002XXH is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MX89510 PP LNP* THERMOCOMP* MX89510 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated |