Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
NYCOA 1417HS PA 6 impact modified, heat stabilized, medium high impact strengthInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY XP4025 ASA+PC (Asia Pacific) ASA+PC blend. Weatherable, injection grade. Available in a wide range of colors and is recommended for unpainted exterior applications. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 1.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.18 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Ineos Nova 240 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Extremely high impact with good flexural stiffness, Custom colorsApplications: Injection molding, Small appliances, Photographic equipmentPerformance grades of polystyrene are engineered to have spe.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Ineos HP53-25-155 HDPE HP53-25-155 is a high performance, high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blow molding equipment, specifically where appli.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Kostat BK-STAT 7048BK ABS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature -30.0 °C |
3.18 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722. |
|||
Izod Impact, Notched | 1.70 J/cm @Thickness 3.20 mm |
3.18 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature -30.0 °C |
3.18 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 LNP* THERMOCOMP* PF00C is a compound based on Nylon 6 resin containing 60% Glass Fiber. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermotuf VF002 PA 66 LNP THERMOTUF* VF002 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PB302G50 Nylon 6, 50% Glass Fiber 50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Toyobo TS501 PPS, 50% Glass Fiber Reinforced Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber A CHEMICALLY COUPLED 30% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPC301G2 Polypropylene, 10% Glass Fiber 10% glass fibers reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Toyobo T-422T Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughnessInformation provided by Toyobo Co., Ltd |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA250G60W , 62% Glass Fiber Reinforced PA66, DAM High strength, weather resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Adell AJ-34 Nylon 66, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | Wet; ASTM D256 |
Asahi Kasei Leona® 14G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
Adell AI-30 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY FXW751SK ASA+PC Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin |
|||
Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF OF006I PPS - Linear LNP THERMOTUF* OF006I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 1.70 J/cm @Temperature 23.0 °C |
3.18 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH308G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |