| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
| Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.250 % | 0.250 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 1.0 % | 1.0 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 8.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| Melt Index of Compound | 7.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 48.0 MPa | 6960 psi | Type I, 50 mm/min; ASTM D638 |
| 48.0 MPa | 6960 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 |
| 62.0 MPa | 8990 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 49 % | 49 % | Type I, 50 mm/min; ASTM D638 |
| 77 % | 77 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 4.2 % | 4.2 % | Type I, 50 mm/min; ASTM D638 |
| 4.2 % | 4.2 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.68 GPa | 389 ksi | 5 mm/min; ASTM D638 |
| 2.90 GPa | 421 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 78.0 MPa | 11300 psi | 2 mm/min; ISO 178 |
| 95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.70 GPa | 392 ksi | 2 mm/min; ISO 178 |
| 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
| 0.500 J/cm @Temperature -30.0 °C |
0.937 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
| 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.70 J/cm² | 8.09 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 43.0 J @Temperature 23.0 °C |
31.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 89.0 °C @Thickness 3.20 mm |
192 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ASTM D1525 |
| 108 °C | 226 °F | Rate B/50; ISO 306 | |
| 109 °C | 228 °F | Rate B/120; ISO 306 |