| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched |
1.70
J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
3.18
ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
|
Premix Thermoplastics PRE-ELEC® ESD 7200
PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific)
Reinforced PC/ABS with high stiffness and low CTE.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
|
|||
| Izod Impact, Notched |
>=
1.70
J/cm @Temperature 23.0 °C |
>=
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
|
NIZHNEKAMSKNEFTEKHIM PE 6752G (526H7) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific)
LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Ineos Nova 240 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Extremely high impact with good flexural stiffness, Custom colorsApplications: Injection molding, Small appliances, Photographic equipmentPerformance grades of polystyrene are engineered to have spe..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Kostat BK-STAT 7048BK ABS Compound
BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature -30.0 °C |
3.18
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics NORYL WCV063 PPE+SEBS+Polyolefin (Europe-Africa-Middle East)
Flexible, non-halogenated FR, mPPE extrusion grade material for evaluation in automotive wire coating applications requiring ISO6722.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature -40.0 °C |
3.18
ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific)
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"".
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature -30.0 °C |
3.18
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature -30.0 °C |
3.18
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP STAT-LOY A3000LTH ABS
LNP* STAT-LOY* A3000LTH is a compound based on ABS resin. Added features of this material include: Transparent, Antistatic, Formulation Locked.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Asia Pacific)
LNP* Thermocomp* PF00C is a compound based on Nylon 6 resin containing Glass Fiber.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.Information provided by Vyncolit, a Sumitomo Bak Group
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA
LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermotuf VF002 PA 66
LNP THERMOTUF* VF002 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermotuf VF002 PA 66 (Asia Pacific)
LNP THERMOTUF* VF002 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram PB302G50 Nylon 6, 50% Glass Fiber
50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram PlusTek PA4801G6 Nylon 6.6, 30% Glass Fiber Reinforced, PTFE lubricated
30% glass fiber reinforced, PTFE lubricated polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Toyobo TS501 PPS, 50% Glass Fiber Reinforced
Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram RamOfin PPC301G2 Polypropylene, 10% Glass Fiber
10% glass fibers reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Adell AI-10 Nylon 66, Impact Modified
Data provided by Adell Plastics, Inc.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Adell AJ-14 Nylon 66, 20% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Ineos Nova Zyntar® 351 High Performance Flame Retardant Polystyrene
(discontinued **)
High Vicat and heat reflection temperature, Custom colorsApplications: Injection molding, Gas-assist injection molding, Structural foam, TV cabinets, Electronic enclosuresThis is an impact grade of ..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics GELOY FXW751SK ASA+PC
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram RamOfin PPH308G8 Polypropylene, 40% Glass Fiber
40% glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||