| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific)
Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC
LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.18
ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
|
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Shell Carilon® DB6G6P30 Polyketone, Lubricated, Glass-Reinforced, Injection Molding Grade
(discontinued **)&l
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DA6P2L10 is a high-performance lubricated injection molding grade with mechanical properties which ..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
(Unverified Data**)
Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Ineos Nova 240 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Extremely high impact with good flexural stiffness, Custom colorsApplications: Injection molding, Small appliances, Photographic equipmentPerformance grades of polystyrene are engineered to have spe..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
IDI Composites 46-09 Thermoset Polyester, Molding
Abrasion resistant, electrical grade material with V-O flame resistance and moderate strength.Data provided by the manufacturer.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
|
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature -30.0 °C |
3.18
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature -30.0 °C |
3.18
ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6
LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics LNP Thermotuf VF002 PA 66 (Asia Pacific)
LNP THERMOTUF* VF002 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics Noryl 534 PPE+PS
High heat, unreinforced.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram PB302G50 Nylon 6, 50% Glass Fiber
50% glass fiber reinforced, UV and heat stabilized polyamide approved and listed by W.R.C potable water and NSF/ANSI61 internationalInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ISO 180 |
|
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Toyobo TS401 HS PPS, 40% Glass Fiber Reinforced
Key Feature: High toughness, high flow. Features high weld strength.High performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology d..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram PlusTek PA840G6 Nylon 6.6, 30% Glass Fiber
30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber
A CHEMICALLY COUPLED 30% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris..
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
|
Polyram RamOfin PPC301G2 Polypropylene, 10% Glass Fiber
10% glass fibers reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Toyobo T-422T Nylon, Mineral-Reinforced
Key Feature: High heat distortion and good toughnessInformation provided by Toyobo Co., Ltd
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
E-Polymers TEKAMID® TA250G60W , 62% Glass Fiber Reinforced PA66, DAM
High strength, weather resistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Adell AJ-14 Nylon 66, 20% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
|
|||
| Izod Impact, Notched |
1.70
J/cm @Temperature 23.0 °C |
3.18
ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
|
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**)
Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched | 1.70 J/cm | 3.18 ft-lb/in | ASTM D256 |
|
Adell AI-30 Nylon 66, Impact Modified
Data provided by Adell Plastics, Inc.
|
|||