Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH
(d AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATAMID 12 H FE85 Nylon 12 Base Magnetizable Compound
(discontinued **) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Izod Impact, Notched | 0.310 - 2.51 J/cm | 0.580 - 4.70 ft-lb/in | Average value: 0.617 J/cm Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 A |
Metabolix Mirel™ F1006 Injection Molding Grade PHA Bioplastic Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 A |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 9405H-1 Glass Filled Electrical Encapsulation Grade Epoxy E-9504H-1 is glass fiber filled epoxy molding compound designed for encapsulation of delicate electrical components as well as large coils. Excellent thermal shock, moldability, and retention of ele.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Asia Pacific) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific) LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EFN4230 PPE+PS (Asia Pacific) PPE+PS high heat transparent grade |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature -30.0 °C |
0.581 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6 (Europe-Africa-Middle East) Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 22.8 °C |
0.580 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene MFP 22KA2 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-96 Compression Molded PEEK Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Ensinger Tecatron® XP-85 Compression Molded PPS Compound, with 30% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.580 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339M30CL Mica Reinforced Coupled |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | ASTM D256 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.310 J/cm | 0.581 ft-lb/in | |
Abatron AboCast 50-3/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months. |
|||
Izod Impact, Notched | 0.310 - 5.30 J/cm | 0.581 - 9.93 ft-lb/in | Average value: 0.762 J/cm Grade Count:14 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.310 J/cm @Temperature 23.0 °C |
0.581 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 501 HC Bioriented Film Polypropylene Applications: High stiffness; barrier films for conversionInformation provided by Braskem |