Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ensinger Tecapeek® XP-96B Compression Molded PEEK, Unfilled, Black Pigmented.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Filler Content 0.00 %
0.00 %
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 101
101
ASTM D785
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength 95.1 MPa
13800 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
4.5 %
4.5 %
Flexural Strain; ASTM D790
Tensile Modulus 5.31 GPa
770 ksi
ASTM D638
Flexural Strength 154 MPa
22300 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Compressive Strength 133 MPa
19300 psi
10% Deformation; ASTM D695
Compressive Modulus 2.48 GPa
360 ksi
ASTM D695
Izod Impact, Notched 0.310 J/cm
0.580 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Heat Distortion Temperature 149 °C
300 °F
ASTM D648
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: