Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 290 MPa | 42100 psi | |
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Polyplastic Armamid® PA GF50-1 Nylon 6, 50% Glass Fiber High stiffnessInformation provided by PolyPlastic Group. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Nilit FRIANYL A63 GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | <= 290 MPa | <= 42100 psi | ISO 178 |
Polykemi AB SCANAMID 66 A12^ F50 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 290 MPa | <= 42100 psi | ISO 178 |
Polykemi AB SCANMID 6 B11^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 290 MPa @Temperature 23.0 °C |
42100 psi @Temperature 73.4 °F |
ISO 178 |
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Strength | 290 MPa | 42100 psi | |
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Strength | 290 MPa | 42100 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Strength | 290 MPa @Temperature 23.0 °C |
42100 psi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel |
|||
Flexural Strength | 290 MPa | 42100 psi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 140 DUS008 000000 Nylon 6, 40% Glass Fiber PA 6, 40% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Flexural Strength | 290 MPa @Strain 4.00 % |
42100 psi @Strain 4.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 140 H2.0 DUS008 900051 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 40% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Flexural Strength | 290 MPa | 42100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OE008A PPS - Branched (Europe-Africa-Middle East) LNP* Stat-kon* OC-1008 is a compound based on PPS - Branched resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Polyram PlusTek PA303G6BK16 Nylon 6.6, 30% Glass Fiber reinforced, Heat Stabilized, Hydrolysis Resistant 30% Glass fiber reinforced, heat stabilized, hydrolysis resistant, improved surface finish Nylon 6.6. Approved and listed by W.R.A.S.Information provided by Polyram. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Polyram PlusTek RA303G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced, heat stabilized, and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance.. |
|||
Flexural Strength | 290 MPa @Temperature 23.0 °C |
42100 psi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® FGFE5171 NC010C Nylon 66
(Unverified Data**) Zytel® FGFE5171 NC010C is a 33% glass filled nylon 66 resin. It has been developed for consideration into applications such as parts for the food industry.Information provided by DuPont Performance.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ISO 178 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |
|||
Flexural Strength | 290 MPa | 42100 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |
|||
Flexural Strength | 290 MPa | 42100 psi | 5 mm/min; ISO 178 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |