Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 6
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby tools, gears, covers of electric appliances, cooling skrews of blowers, electromotors, carrying parts in the automotive industry.Delivered in natural and in the full RAL colour scale.PA 6 for injection moulding, lightly impacted.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
Viscosity Measurement 0.40 - 1.2
0.40 - 1.2
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
Melt Flow 1.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
1.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 14.5 GPa
2100 ksi
Flexural Strength 290 MPa
42100 psi
Flexural Modulus 12.5 GPa
1810 ksi
Charpy Impact Unnotched 8.50 J/cm²

@Temperature -20.0 °C
40.4 ft-lb/in²

@Temperature -4.00 °F
9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.50 J/cm²

@Temperature -20.0 °C
7.14 ft-lb/in²

@Temperature -4.00 °F
1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Vicat Softening Point 210 °C
410 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Comparative Tracking Index 575 V
575 V
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
Mold Temperature 90.0 - 100 °C
194 - 212 °F
Drying Temperature 90.0 °C
194 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 90.0 - 150 MPa
13100 - 21800 psi