Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 135 MPa | 19600 psi | ASTM D790 |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ASTM D790 |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Flexural Strength | 135 MPa | 19600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Flexural Strength | 135 MPa | 19600 psi | |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Radici Radilon® ACP300 K (dry) Nylon 66 Heat stabilized mineral filledInformation provided by Radici group. |
|||
Flexural Strength | 135 MPa | 19600 psi | |
Plastcom SLOVALEN PH 49 GF 30 LW PP, 30% glass fibre, coupling agents, laser writer FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties and contains modificator for laser labeling of fini.. |
|||
Flexural Strength | 135 MPa | 19600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Nilit FRIANYL B63 HS-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 135 MPa | 19600 psi | |
Lehmann & Voss LUVOCOM® 1105-7777 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Isotropic shrinkage characteristics.Emergency running property.Information provided by Leh.. |
|||
Flexural Strength | 135 MPa | 19600 psi | |
Lehmann & Voss LUVOCOM® 1301-7329/GY PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 135 MPa | 19600 psi | DIN 54352 |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Dry Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Strength | 135 MPa | 19600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS DATA ON BK1005 ONLY. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT (Asia Pacific) LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Styrolution Luran® 378 P Crystal Clear Transparent SAN Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Strength | 135 MPa | 19600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Solvay TECHNYL® A 216 S30 PA66, 30% glass spheres, DRY Description: Polyamide 66, reinforced with 30% of glass spheres, for injection molding.Available in: EuropeProduct Applications: TECHNYL® A 216 S30 is used in all sectors of industry, offering an.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Polyram PlusTek PA340S05 Nylon 6.6 for Injection Molding, 5% Glass-beads Reinforced, Heat Stabilized 5% Glass-beads reinforced Nylon 6.6, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 135 MPa | 19600 psi | ASTM D790 |
Polyram PlusTek RA116 Nylon 6.6, Injection Molding polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 135 MPa @Thickness >=1.50 mm |
19600 psi @Thickness >=0.0591 in |
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola Etronax MF G Phenolic, Cotton Fabric Reinforcement, Black, Sheets Description: Exclusively for mechanical applications. Impact-resistant. Resistant to mechanical wear and noise-reducing. The graphite content causes low friction. Well suited for parts where there a.. |
|||
Flexural Strength | >= 135 MPa | >= 19600 psi | Perpendicular to laminations; IEC 1212-2 5.1 |
Hippe PF CP 201 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical applications. Used in mechanical properties better than other PF CP types. Poor electrical properties under normal humidity. Also available in hot-punching versions.Information.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C467-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |
|||
Flexural Strength | 135 MPa | 19600 psi | 10mm/min; ASTM D790 |
BLUESTAR PBT 403M-G20 20% Glass Filled PBT, injection molding grade, 20% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorable.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 135 MPa | 19600 psi | ASTM D790 |
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North.. |
|||
Flexural Strength | 135 MPa | 19600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has .. |