Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® ACP300 K (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Mineral Filled
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® ACP300 K (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat stabilized mineral filledInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527-1/2
Elongation at Break 6.8 %
6.8 %
ISO 527-1/2
Tensile Modulus 5.05 GPa
732 ksi
ISO 527-1/2
Flexural Strength 135 MPa
19600 psi
ISO 178
Flexural Modulus 4.50 GPa
653 ksi
ISO 178
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO 75/2Af
Vicat Softening Point 245 °C
473 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Users viewing this material also viewed the following: