| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 | 
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050           cm/cm @Thickness 3.20 mm | 0.0030 - 0.0050           in/in @Thickness 0.126 in | SABIC Method | 
| Linear Mold Shrinkage, Transverse | 0.0030 - 0.0050           cm/cm @Thickness 3.20 mm | 0.0030 - 0.0050           in/in @Thickness 0.126 in | SABIC Method | 
| Melt Flow | 37           g/10 min @Load 5.00 kg, Temperature 260 °C | 37           g/10 min @Load 11.0 lb, Temperature 500 °F | ASTM D1238 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 121 | 121 | ISO 2039-2 | 
| Hardness, H358/30 | 116 MPa | 16800 psi | ISO 2039-1 | 
| Tensile Strength at Break | 85.0 MPa | 12300 psi | Type I, 5 mm/min; ASTM D638 | 
| 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 85.0 MPa | 12300 psi | Type I, 5 mm/min; ASTM D638 | 
| 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 | 
| 3.2 % | 3.2 % | 5 mm/min; ISO 527 | |
| Elongation at Yield | 3.0 % | 3.0 % | Type I, 5 mm/min; ASTM D638 | 
| Tensile Modulus | 4.70 GPa | 682 ksi | 1 mm/min; ISO 527 | 
| 4.90 GPa | 711 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 135 MPa | 19600 psi | 2 mm/min; ISO 178 | 
| 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Yield Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 | 
| Flexural Modulus | 4.25 GPa | 616 ksi | 2 mm/min; ISO 178 | 
| 4.30 GPa | 624 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 | 
| 0.600           J/cm @Temperature -30.0 °C | 1.12           ft-lb/in @Temperature -22.0 °F | ASTM D256 | |
| Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 | 
| 4.80           J/cm @Temperature -30.0 °C | 8.99           ft-lb/in @Temperature -22.0 °F | ASTM D4812 | |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A | 
| 6.00           kJ/m² @Temperature -30.0 °C | 2.86           ft-lb/in² @Temperature -22.0 °F | 80*10*4; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 30.0 kJ/m² | 14.3 ft-lb/in² | 80*10*4; ISO 180/1U | 
| Dart Drop, Total Energy | 8.00           J @Temperature -30.0 °C | 5.90           ft-lb @Temperature -22.0 °F | ASTM D3763 | 
| 15.0           J @Temperature 23.0 °C | 11.1           ft-lb @Temperature 73.4 °F | ASTM D3763 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear, Parallel to Flow | 40.0           µm/m-°C @Temperature -40.0 - 40.0 °C | 22.2           µin/in-°F @Temperature -40.0 - 104 °F | ASTM E 831 | 
| CTE, linear, Transverse to Flow | 75.0           µm/m-°C @Temperature -40.0 - 40.0 °C | 41.7           µin/in-°F @Temperature -40.0 - 104 °F | ASTM E 831 | 
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | ISO 8302 | 
| Deflection Temperature at 0.46 MPa (66 psi) | 134           °C @Thickness 3.20 mm | 273           °F @Thickness 0.126 in | unannealed; ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 126           °C @Thickness 3.20 mm | 259           °F @Thickness 0.126 in | unannealed; ASTM D648 | 
| 128           °C @Thickness 6.40 mm | 262           °F @Thickness 0.252 in | unannealed; ASTM D648 |