Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC LNP* LUBRICOMP* DFP36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFI14 PC LNP* Lubricomp* DFI14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 2% Silicone. Added features include: Internally Lubricated. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA 12 (Asia Pacific) LNP* Lubricomp* SP003 is a compound based on Nylon 12 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC (Asia Pacific) LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Easy Molding. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON EE005E PEI LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific) LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific) LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP EC005 PEI (Asia Pacific) LNP THERMOCOMP* EC005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp RF005 PA 66 (Asia Pacific) LNP* Thermocomp* RF005 is a compound based on Nylon 66 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp WX01910L PBT LNP* Thermocomp* WX01910L is a compound based on Thermoplastic Polyester containing Proprietary Fillers. Characteristics of this grade are: Low Extractable.This data was supplied by SABIC-IP for t.. |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon DX96690 PC LNP STAT-KON* DX96690 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the America.. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP NF002 PC+ABS LNP THERMOCOMP* NF002 is a compound based on PC+ABS resin containing 10% Glass Fiber. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Impact Test | 7.00 J | 5.16 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOTUF VX99810 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |
|||
Impact Test | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp UC008S PPA LNP* Thermocomp* UC008S is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for.. |