Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Impact Test | 15.0 J @Temperature -30.0 °C |
11.1 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplication.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC LNP LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing 20% Milled Glass, 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON CD0001 PS LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp LF003E PEEK (Asia Pacific) LNP* Thermocomp* LF003E is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Thermocomp YF005 LNP* Thermocomp* YF005 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific) Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon DS0029 PC LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific) LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Impact Test | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated. |
|||
Impact Test | 15.0 J | 11.1 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific) LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |