Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RX06422 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RX06422 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
1.58 g/cc
0.0571 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0018 cm/cm

@Time 86400 sec
0.0018 in/in

@Time 24.0 hour
ASTM D955
0.0018 cm/cm

@Time 86400 sec
0.0018 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ASTM D955
0.0022 cm/cm

@Time 86400 sec
0.0022 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 254 MPa
36800 psi
ASTM D638
256 MPa
37100 psi
ISO 527
Elongation at Break 1.9 %
1.9 %
ISO 527
1.9 %
1.9 %
ASTM D638
Tensile Modulus 16.89 GPa
2450 ksi
50 mm/min; ASTM D638
18.38 GPa
2666 ksi
1 mm/min; ISO 527
Flexural Strength 370 MPa
53700 psi
ISO 178
374 MPa
54200 psi
ASTM D790
Flexural Modulus 14.16 GPa
2054 ksi
ASTM D790
15.55 GPa
2255 ksi
ISO 178
Izod Impact, Notched 3.84 J/cm
7.19 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1A
38.0 kJ/m²

@Temperature -40.0 °C
18.1 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 89.0 kJ/m²
42.4 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 J
11.1 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 15.0 J
11.1 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 18.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
18.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 67.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
67.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.4 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 258 °C
496 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 253 °C
487 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
241 °C

@Thickness 3.20 mm
466 °F

@Thickness 0.126 in
unannealed; ASTM D648