SABIC Innovative Plastics LNP THERMOCOMP DX08028 PC Copolymer (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DX08028 PC Copolymer (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* DX08028 is a compound based on PC Copolymer resin, containing proprietary filler(s). Added features include: Heat Stabilized, FDA Compliant Raw Materials, Metal Detectable.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
SABIC Method
Melt Index of Compound 5.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
50 mm/min; ISO 527
Tensile Strength, Yield 56.0 MPa
8120 psi
50 mm/min; ISO 527
Elongation at Break 75 %
75 %
50 mm/min; ISO 527
Elongation at Yield 6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 85.0 MPa
12300 psi
2 mm/min; ISO 178
Flexural Modulus 2.20 GPa
319 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 34.0 kJ/m²
16.2 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
261 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af