Category | Polymer , Thermoplastic , Polystyrene (PS) , Syndiotactic Polystyrene (SPS) |
Manufacturer | PolyOne Corporation |
Trade Name | Edgetek® |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | PolyOne Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.25 g/cc | 1.25 g/cc | ISO 1183 |
Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ISO 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 120 MPa | 17400 psi | Type I, 5.0 mm/min; ISO 527 |
Elongation at Break | 1.3 % | 1.3 % | Type I, 5.0 mm/min; ISO 527 |
Tensile Modulus | 9.00 GPa | 1310 ksi | Type I, 5.0 mm/min; ISO 527 |
Flexural Strength | 170 MPa | 24700 psi | ISO 178 |
Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
Charpy Impact Unnotched | 3.40 J/cm² | 16.2 ft-lb/in² | ISO 179 |
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 230 °C @Thickness 3.18 mm |
446 °F @Thickness 0.125 in |
Unannealed; ISO 75-2/A |
Flammability, UL94 | HB | HB | UL 94 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 270 - 320 °C | 518 - 608 °F | |
Mold Temperature | 80.0 - 150 °C | 176 - 302 °F | |
Drying Temperature | 80.0 °C | 176 °F | |
Dry Time | 2.00 hour | 2.00 hour |
Descriptive Properties | Value | Comments |
---|---|---|
Appearance | Natural Color | |
Filler / Reinforcement | Glass Fiber Reinforcement | |
Forms | Pellets | |
Generic Material | SPS | |
Generic Name | Syndiotactic Polystyrene (SPS) | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America |