Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
PolyOne LubriOne™ AT-000/15T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | ASTM D955 |
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D955 |
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B65B0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
LATI Latan 13 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
LATI Latan 2 POM Polyoxymethylene (POM). Unfilled. High viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Linear Mold Shrinkage, Flow | 0.0195 - 0.023 cm/cm | 0.0195 - 0.023 in/in | |
LATI Latan 23UV POM Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by .. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
LATI Latan 9 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
LATI Latilub 73/13-01M POM, Molybdenum disulphide Filled Self-lubricating product based on Polyoxymethylene (POM). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati In.. |
|||
Linear Mold Shrinkage, Flow | 0.020 - 0.023 cm/cm | 0.020 - 0.023 in/in | |
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Linear Mold Shrinkage, Flow | 0.021 - 0.023 cm/cm | 0.021 - 0.023 in/in | SABIC Method |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK (Europe-Africa-Middle East) LNP*LUBRICOMP* LFL36 is a compound based on Polyetheretherketone resin containing Glass Fiber, PTFE.
Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RFL46 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL46 is a compound based on PA66 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004 is a compound based on Nylon 66 resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004S is a compound based on Nylon 66 resin containing PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.023 cm/cm @Thickness 2.30 - 4.60 mm |
0.015 - 0.023 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.023 cm/cm @Thickness 3.20 mm |
0.015 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.023 cm/cm @Thickness 2.30 - 4.60 mm |
0.015 - 0.023 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.023 cm/cm @Thickness 2.30 - 4.60 mm |
0.015 - 0.023 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.023 cm/cm @Thickness 3.20 mm |
0.015 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm @Thickness 3.20 mm |
0.017 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 315 PBT (Asia Pacific) General purpose polyester. Fully imported product from USA |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm @Thickness 3.20 mm |
0.017 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® VAC3001 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm @Thickness 3.20 mm |
0.017 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® VAC3003 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1606-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.019 - 0.023 cm/cm | 0.019 - 0.023 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1627-GY1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |