PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Recommended for interior applications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
15 sec; ASTM D2240
75
75
ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
510 mm/min; ASTM D638
Tensile Strength 5.03 MPa

@Strain 100 %
730 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 420 %
420 %
510 mm/min; ASTM D638
Tear Strength 49.0 kN/m
280 pli
Die C, 510 mm/min; ASTM D624
Compression Set 30 %

@Temperature 23.0 °C,
Time 79200 sec
30 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.0986 GPa
14.3 ksi
ASTM D1043
0.310 GPa

@Temperature -47.0 °C
45.0 ksi

@Temperature -52.6 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -46.7 °C
-52.1 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 174 - 179 °C
345 - 354 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features General Purpose
Low Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose