Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible B6500 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
15 sec; ASTM D2240
65
65
ASTM D2240
Tensile Strength at Break 10.3 MPa
1490 psi
510 mm/min; ASTM D638
Tensile Strength 3.62 MPa

@Strain 100 %
525 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 460 %
460 %
510 mm/min; ASTM D638
Tear Strength 38.5 kN/m
220 pli
Die C, 510 mm/min; ASTM D624
Compression Set 22 %

@Temperature 23.0 °C,
Time 79200 sec
22 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.0241 GPa
3.50 ksi
ASTM D1043
0.310 GPa

@Temperature -55.0 °C
45.0 ksi

@Temperature -67.0 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -51.1 °C
-60.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
ALL; UL 94
Processing Properties Metric English Comments
Melt Temperature 168 - 174 °C
334 - 345 °F
188 - 199 °C
370 - 390 °F
Descriptive Properties Value Comments
Features General Purpose
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose
Users viewing this material also viewed the following: