Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | ASTM D955 |
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LCG2007 PC (Asia Pacific) |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm @Thickness 3.18 mm |
0.0015 - 0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | Injection molding; ISO 2577 |
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | |
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0045 cm/cm | 0.0015 - 0.0045 in/in | |
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
LATI Latilub 87/28-15T K/20 PC, 20% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF15 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC3008A PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC3008A compound is a 30% carbon fiber/glass/mineral filled, static dissipative, foamable resin. UL94 V1 rated. Property values at 20% weight reduction, 0.250"" wall. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1508 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC1508 compound is a static dissipative NORYL resin. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0017 cm/cm @Time 86400 sec |
0.0015 - 0.0017 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66 LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PES GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Good Wear Resistance, Low Extractables, Lubricat.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | GB/T 15585-1995 |
Sichuan Deyang Haton® hMR60 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched (Europe-Africa-Middle East) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP ZF004 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004 is a compound based on PPE+PS Blend resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm @Thickness 4.00 mm |
0.0015 - 0.0035 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | on Tensile Bar; E2P method |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | ASTM D955 |
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | ISO 294 |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL CN5260 PPE+PS (Asia Pacific) 50% filled FR high modulus PPE/PS blend |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | |
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF40 BK 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |