Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sichuan Deyang Haton® hMR60 Polyphenylene Sulfide, Glass & Mineral Reinforced

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer Sichuan Deyang Chemical Co. Ltd.
Trade Name Haton®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sichuan Deyang Haton® hMR60 Polyphenylene Sulfide, Glass & Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Physical Properties Metric English Comments
Density 1.97 g/cc
0.0712 lb/in³
GB/T 1033.1-2008
Water Absorption 0.020 %
0.020 %
GB/T 1034-2008
Linear Mold Shrinkage, Flow 0.0015 cm/cm
0.0015 in/in
GB/T 15585-1995
Linear Mold Shrinkage, Transverse 0.0048 cm/cm
0.0048 in/in
GB/T 15585-1995
Mechanical Properties Metric English Comments
Hardness, Rockwell L 107
107
GB/T 3398.2-2008
Tensile Strength 164 MPa
23800 psi
GB/T 1040.2-2006
Elongation at Break 1.4 %
1.4 %
GB/T1040.2-2006
Flexural Strength 244 MPa
35400 psi
GB/T 9341-2008
Flexural Modulus 17.5 GPa
2540 ksi
GB/T 9341-2008
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
GB/T 1843-2008
Izod Impact, Unnotched (ISO) 59.0 kJ/m²
28.1 ft-lb/in²
GB/T 1843-2008
Thermal Properties Metric English Comments
Melting Point 280 °C
536 °F
GBT/T 19466.3-2004
Deflection Temperature at 1.8 MPa (264 psi) 270 °C
518 °F
GB/T 1634.2-2004
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+16 ohm-cm
1.60e+16 ohm-cm
GB/T1410-2006
Surface Resistivity per Square 4.00e+15 ohm
4.00e+15 ohm
GB/T1410-2006
Dielectric Constant 5.0
5.0
GB/T 1409-2006
Dielectric Strength 14.0 kV/mm
356 kV/in
GB/T1408.1-2006
Dissipation Factor 0.0010
0.0010
GB/T 1409-2006