Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0015 - 0.0030 cm/cm

@Thickness 3.18 mm
0.0015 - 0.0030 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cm

@Thickness 3.18 mm
0.0080 - 0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.1 MPa
9300 psi
5.1 mm/min; ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Tensile Modulus 4.69 GPa
680 ksi
5.1 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
1.3 mm/min; ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.70 J/cm

@Temperature 23.0 °C
5.06 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 3.18 mm
V-0

@Thickness 0.125 in
Internal Method; UL 94
Descriptive Properties Value Comments
Features Amorphous
Flame Retardant
Filler / Reinforcement GlassCarbon Fiber Reinforcement
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Business Equipment
Electrical Housing