Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 - 1.53 g/cc | 0.0379 - 0.0553 lb/in³ | Average value: 1.14 g/cc Grade Count:156 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Density | 1.33 - 1.53 g/cc | 0.0480 - 0.0553 lb/in³ | Average value: 1.43 g/cc Grade Count:18 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Density | 1.22 - 1.53 g/cc | 0.0441 - 0.0553 lb/in³ | Average value: 1.35 g/cc Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 0.940 - 1.53 g/cc | 0.0340 - 0.0553 lb/in³ | Average value: 1.16 g/cc Grade Count:60 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Density | 1.15 - 1.53 g/cc | 0.0415 - 0.0553 lb/in³ | Average value: 1.29 g/cc Grade Count:98 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.11 - 1.53 g/cc | 0.0401 - 0.0553 lb/in³ | Average value: 1.27 g/cc Grade Count:57 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 410 Rigid PVC, Extrusion Clic channels |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 218 Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 321 Rigid PVC, Extrusion Lead Free Profiles |
|||
Density | 1.50 - 1.53 g/cc | 0.0542 - 0.0553 lb/in³ | Fusor 2200 |
Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive Fusor® 2200/2201 is a black equal-mix, twocomponent, paste urethane adhesive system. Fusor 2200/2201 adhesive bonds FRP, SMC, and other plastics with little surface preparation where bond strengt.. |
|||
Density | 1.03 - 1.53 g/cc | 0.0372 - 0.0553 lb/in³ | |
Trelleborg Offshore Vikotherm™ 73185 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Density | 1.50 - 1.53 g/cc | 0.0542 - 0.0553 lb/in³ | Laminate |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 82 Flexible PVC, Sheathing General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 93 Flexible PVC, Insulation Lead Free General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 0753 Flexible PVC, Flame Retardant Insulation Lead Free General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 86/1 Flexible PVC, Flame Retardant Insulation Lead Free Power cables |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 75/1 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 85 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 85 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 85/1 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/25 Halogen Free PVC Insulation; very low thickness |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4022 Halogen Free PVC General purpose |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1184 |
Fainplast Compounds R 218 Rigid PVC, Extrusion Shutters and shiny profiles |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4021 Halogen Free PVC General purpose |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 018/25 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Insulation; very low thicknessInformation provided by Fainplast Compounds |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1184 |
Fainplast Compounds HG 82 Flexible PVC, Sheathing for High Temperatures Sheathing general purposes |
|||
Density | 1.44 - 1.53 g/cc | 0.0520 - 0.0553 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Density | 1.09 - 1.53 g/cc | 0.0394 - 0.0553 lb/in³ | Average value: 1.23 g/cc Grade Count:23 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Density | 1.49 - 1.53 g/cc | 0.0538 - 0.0553 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 90/2 Flexible PVC, Flame Retardant Insulation General purposes |