| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | STN EN ISO 1183-1 |
|
Plastcom PLASTAMID® 6 GF 30 002 TS PA6 reinforced with glass fiber, heat stabilized
PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used for holders of hand tools, hobby tools, gear wheel..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | STN 64 0111 |
|
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization
FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools...
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Europe-Africa-Middle East)
CYCOLOY MC5220 is a 20% glass reinforced PC+ABS blend for injection moulding purposes.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | |
|
Pyrotek TS-83 Thermoset Electrical Insulation Product (Nema Grade: LE)
Linen reinforcement, Phenolic resin, Tan / Black color. Good electrical and high mechanical strength. Moisture resistant.Information provided by Pyrotek.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
Polykemi AB POLYform POM C M20 AS4 Polyoxymethylene, Antistatic
Information provided by Polykemi AB
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Lexan® FXR123R PC (Europe-Africa-Middle East)
Lexan FXR123R Resin
|
|||
| Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RST 171 Rigid PVC, Extrusion Lead Free
Various transparent profiles
|
|||
| Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ASTM D792 |
|
KYDEX® 6185 Thermoplastic Sheet
High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP Lubricomp UL004AS PPA (Europe-Africa-Middle East)
Internally lubricated Polyphthalamide compound, countaining PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Density |
1.33
g/cc <br>@Diameter 0.360 mm
|
0.0480
lb/in³ <br>@Diameter 0.0142 in
|
Product yield of 7370 m/kg. |
|
Shakespeare Sanstat® CN125 .36mm Nylon 66 Monofilament
Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by ..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 GF/M25HS L BK 25% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by Weight and Mineral Filler, 25% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
|
Techmer ES Luriblend® PC CF10 TL10 BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific)
LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
|
Techmer ES Electrablend® ABS SS16 FR BK 16% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 16% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi..
|
|||
| Density |
1.33
g/cc <br>@Temperature 60.0 °C
|
0.0480
lb/in³ <br>@Temperature 140 °F
|
|
|
Solvay Aluminum Sulfate Low Iron Technical Grade
Description Aluminum Sulfate, Solution, technical grade is a clear, water white to slightly yellow-brown liquid. It complies with the standards of the American Water Works Association B403-98. It ha..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
Unitika A3130HR-25 PA6, 25% Mineral Reinforced, Dry
Information provided by Unitika Ltd.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
Polyram RamOfin PPH308G50 Polypropylene, 50% Glass Fiber, Impact Modified
50% Glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applications.Information provided by Polyram.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | JIS-Z-8807 |
|
Denka REOMER G G5479 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
|
E-Polymers TEKAMID® TA210SG30 Impact Modified, 30% Glass Fiber Reinforced PA66, DAM
30% Glass Fiber reinforced, Impact resistanceInformation provided by E-Polymers Co. Ltd.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
|
E-Polymers TEKANATE™ G720 , 20% Glass Fiber Reinforced Poly Carbonate
20% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
|
Fainplast Compounds KL 84/1 Flexible PVC, Insulation for High Temperatures Lead Free
General purposes flame retardant
|
|||
| Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PK 9220 Flexible PVC, Lead Free
Fencing
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
|
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry)
Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6.
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | |
|
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon R38726R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured SiliconeProduct Use: Flexible heater substrateAppearance: Red colored, high ..
|
|||
| Density | 1.33 g/cc | 0.0480 lb/in³ | |
|
LATI Latigea B02 H6 Bio-Polymer
Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop..
|
|||