Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polycarbonate/Polysulfone Alloy

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polysulfone Alloy , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate/Polysulfone Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.22 - 1.53 g/cc
0.0441 - 0.0553 lb/in³
Average value: 1.35 g/cc Grade Count:7
Filler Content 10.0 - 20.0 %
10.0 - 20.0 %
Average value: 16.7 % Grade Count:3
Water Absorption 0.180 - 0.200 %
0.180 - 0.200 %
Average value: 0.193 % Grade Count:3
Linear Mold Shrinkage 0.00150 - 0.0100 cm/cm
0.00150 - 0.0100 in/in
Average value: 0.00450 cm/cm Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.5 - 138 MPa
9500 - 20000 psi
Average value: 95.2 MPa Grade Count:7
Elongation at Break 1.50 - 100 %
1.50 - 100 %
Average value: 18.4 % Grade Count:7
Modulus of Elasticity 2.34 - 11.0 GPa
340 - 1600 ksi
Average value: 5.60 GPa Grade Count:7
Flexural Yield Strength 93.1 - 207 MPa
13500 - 30000 psi
Average value: 142 MPa Grade Count:7
Flexural Modulus 2.62 - 10.7 GPa
380 - 1550 ksi
Average value: 5.33 GPa Grade Count:7
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.839 J/cm Grade Count:7
Izod Impact, Unnotched 3.20 - 5340 J/cm
6.00 - 10000 ft-lb/in
Average value: 8.10 J/cm Grade Count:7
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 149 - 163 °C
300 - 325 °F
Average value: 154 °C Grade Count:7
Flammability, UL94 V-2 - V-0
V-2 - V-0
Grade Count:5
Processing Properties Metric English Comments
Melt Temperature 282 - 327 °C
540 - 620 °F
Average value: 304 °C Grade Count:5
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Average value: 82.2 °C Grade Count:7
Drying Temperature 121 °C
250 °F
Average value: 121 °C Grade Count:5
Moisture Content 0.0200 %
0.0200 %
Average value: 0.0200 % Grade Count:5
Dew Point -28.9 °C
-20.0 °F
Average value: -28.9 °C Grade Count:5
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:7
Users viewing this material also viewed the following: