Polymer Property : Density = 0.0542 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Perstorp Compounds Aminel FX Melamine
Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp ..
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC
LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183/A
Solvay Specialty Polymers Amodel® A-4122 HR WH 117 Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-4122 HR resin is a 22% glass reinforced polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high st..
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
DSM Akulon® K224-TG9/A Nylon 6-45% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP
SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir..
Density 1.50 g/cc
0.0542 lb/in³
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES (Europe-Africa-Middle East)
LNP* Lubricomp* JX91198 is a compound based on Polyethersulfone resin containing Carbon Fiber, Proprietary Lubricant.
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer
LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized.
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific)
LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade
Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Wellman Wellamid® GFX1717-BK1 Nylon 66, 43% Glass Fiber Reinforced, Silicone Lubricated
All information provided by Wellman Engineered Resins.
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Polyram RamSter PF305G6 PBT, 30% Glass Fiber
30% Glass fiber reinforced, PBT for injection molding applications.Information provided by Polyram.
Density 1.50 g/cc
0.0542 lb/in³
Trelleborg Emerson & Cuming Eccobond® A 359 One-Component High Temperature Performance Epoxy Adhesive
Emerson & Cuming A 359 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveAluminum filled, heat curing, epoxy adhesive. Sag resistant. Exceptional thermal and chemical resistance. H..
Density 1.50 - 1.53 g/cc
0.0542 - 0.0553 lb/in³
Laminate
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Tape Form
Material Description: T6T145; Fiber: T300-6KInformation provided by HexCel
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
EMS-Grivory Grivory® XE 5106 (GVL-4H V0) PA*-GF40
Product description: Grivory XE 5106 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf..
Density 1.50 - 1.54 g/cc
0.0542 - 0.0556 lb/in³
ISO R 1183
Fainplast Compounds GA 80/2 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion
Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Ashley Polymers Ashlene® 62M Nylon 66, 40% Mineral reinforced
A 40% mineral reinforced Nylon 66 resin modified for reduced shrinkage.Data provided by the manufacturer
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
Information provided by BASF
Density 1.50 g/cc
0.0542 lb/in³
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® 301-G20F PBT Resin
20% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.50 g/cc
0.0542 lb/in³
Nominal Laminate
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/280H5/AS4-3K
Fiber: AS, Weave: 5HS, 280 g/m2Information provided by HexCel
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.