Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 79
75 - 79
ISO R 868
Tensile Strength at Break >= 12.0 MPa
>= 1740 psi
ISO R 527
Elongation at Break >= 280 %
>= 280 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -31.0 °C
-23.8 °F
Cold Flex; ISO 458/2
Descriptive Properties Value Comments
Thermal Stability (minutes) 140
CEI 20-34/3-2