Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Glass Fiber Filled, Flame Retardant
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retardant ability with an excellent balance of high strength, stiffness and heat distortion temperature.Applications: connectors, terminal blocks, switches and receptacles, coil bobbins, and appliance housingInformation provided by BASF
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.90 %
0.90 %
24 hour; ASTM D570
1.1 %
1.1 %
50% RH; ASTM D570
4.0 %
4.0 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm
0.00762 in/in
1/8" bar
Thermal Properties Metric English Comments
UL RTI, Electrical 130 °C

@Thickness 2.50 mm
266 °F

@Thickness 0.0984 in
746B
UL RTI, Mechanical with Impact 115 °C

@Thickness 2.50 mm
239 °F

@Thickness 0.0984 in
746B
UL RTI, Mechanical without Impact 115 °C

@Thickness 2.50 mm
239 °F

@Thickness 0.0984 in
746B
Processing Properties Metric English Comments
Melt Temperature 250 - 290 °C
482 - 554 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.15 %
<= 0.15 %
Descriptive Properties Value Comments
Color White to gray
Commercial Status North America
Copyright © lookpolymers.com All Rights Reserved