Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Water Absorption 8.1 %
8.1 %
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
23°C/50% R.H.; ISO 62
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ISO 75
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in