Material Notes:
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use, chemical resistance, biocompatibility, and precision extruded tolerances.Very Lubricious - Lowest coefficient of friction of any polymerWorking temperature range 500° F (260° C) to -454° F (–270° C)Chemically Resistant (all common solvents, acids and bases)Chemically InertLow extractableExcellent Dielectric Insulation PropertiesZeus capabilities include:TubingSpecial profilesMonofilamentMultilumenUltra-tight tolerancesFillers: glass, radio-opaque, pigmentsEtching available for bondability
Physical Properties Metric English Comments
Density 2.16 - 2.22 g/cc
0.0780 - 0.0802 lb/in³
ASTM D792
Water Absorption 0.00 %
0.00 %
ASTM D257
Crystallinity >= 90 %
>= 90 %
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 65
50 - 65
ASTM D2240
Tensile Strength, Ultimate 20.0 - 35.0 MPa
2900 - 5080 psi
ASTM D638
Elongation at Break 200 - 550 %
200 - 550 %
ASTM D638
Modulus of Elasticity 0.390 - 0.600 GPa
56.6 - 87.0 ksi
ASTM D638
Flexural Modulus 0.275 - 0.700 GPa
39.9 - 102 ksi
ASTM D790
Coefficient of Friction 0.020 - 0.20
0.020 - 0.20
Thermal Properties Metric English Comments
CTE, linear 126 - 180 µm/m-°C

@Temperature 20.0 °C
70.0 - 100 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.167 - 0.300 W/m-K
1.16 - 2.08 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 327 - 342 °C
621 - 648 °F
Maximum Service Temperature, Air 260 °C
500 °F
Continuous Service
Minimum Service Temperature, Air -270 °C
-454 °F
Glass Transition Temp, Tg 127 °C
261 °F
Decomposition Temperature 400 - 500 °C
752 - 932 °F
ASTM E1131
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.35
1.35
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 - 1.00e+19 ohm-cm
1.00e+14 - 1.00e+19 ohm-cm
ASTM D257
Dielectric Constant 2.1

@Frequency 1.00e+6 Hz
2.1

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 7.44 - 24.0 kV/mm
189 - 610 kV/in
ASTM D149
Descriptive Properties Value Comments
Radiation Resistance (MRad) 1