Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 327 °C | 621 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Melting Point | 327 °C | 621 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Fluorosint® MT-01 PTFE + additives, enhanced grade, compression moulded (ISO Data) Fluorosint MT-01 is an extreme service grade developed specifically for applications where the benefits of PTFE-based materials also require strength, stiffness and stability. Fluorosint MT-01 deliv.. |
|||
Melting Point | 327 °C | 621 °F | DSC |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Melting Point | 327 °C | 621 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® F510 General Purpose Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: General Purpose; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® F710 Chemically Resistant Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: Chemical Resistant; Common in Electrical/ElectronicsInformation provided by Saint Gobain Performance Products. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® F910 FDA Compliant Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: FDA Compliant; Common in Electronics/ElectricalInformation provided by Saint Gobain Performance Products. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.002" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® T-100 Virgin Skived PTFE Sheet (0.250" thick) T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele.. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.015" thick) Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, .. |
|||
Melting Point | 327 °C | 620 °F | ASTM D-3418 |
Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.250" thick) Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, .. |
|||
Melting Point | 327 °C | 621 °F | ASTM D3417 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Melting Point | 327 °C | 621 °F | DIN 53 736 |
Hippe PTFE Good chemical resistance. High thermal stability. Flame resistance. Lowest coefficient of friction among all solid plastics. Very good dielectric properties. Very high weathering resistance.Info.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 206 PTFE, 15/5% Glass/MoS2 Filled Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 215 PTFE, 17% Glass Filled, Blue Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 807 PTFE, 40% Bronze + 5 MoS2 Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 812 PTFE, 46% Bronze, Green Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 826 PTFE, 50% Stainless steel Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 902 PTFE, 1% Conductive filler Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 410 PTFE+ PEEK Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 413 PTFE, 20% PPS Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 816 PTFE, 46% Bronze, Blue Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |