Thermal Properties Metric English Comments
Minimum Service Temperature, Air -270 - -79.0 °C
-454 - -110 °F
Average value: -183 °C Grade Count:26
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Minimum Service Temperature, Air -270 °C
-454 °F
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..