Polymer Property : Modulus of Elasticity = 0.390 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.390 - 0.750 GPa
56.6 - 109 ksi
Average value: 0.599 GPa Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Modulus of Elasticity 0.390 - 0.600 GPa
56.6 - 87.0 ksi
ASTM D638
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..